General Information for Aluminum 356.0, Investment Cast, T6

PropertyDetails
Designation356.0 (Aluminum Association)
ConditionT6 (Solution heat-treated and artificially aged)
UNS NumberA03560
EN NumberEN AC-42000 / EN AC-Al Si7Mg
General Information for Aluminum 356.0, Investment Cast, T6General Information for EN AC-Al Si7Mg

Typical Uses for Aluminum 356.0, Investment Cast, T6

ApplicationDetails
Automotive IndustrySpace frames, wheels, axle and differential housings
Industrial ComponentsPumps, meter housings, intake manifolds
Electronics and Fuel SystemsElectronic cases, fuel pumps
Typical Uses for Aluminum 356.0, Investment Cast, T6Typical Uses for EN AC-Al Si7Mg