Standards with Similar Compositions for Aluminum 356.0, Investment Cast, T6
Country/Region
Standard/Designation
Australia
DA601 to AS 1874
Belgium
AlSi7 to NBN P21-101
Canada
SG70N to CSA HA.10, SG70N to CSA HA.9, SG70P to CSA HA.10, SG70P to CSA HA.9
Czech Republic
424332 to CSN
Europe
EN AC-42000 to CEN EN 1706
France
A-S7G to NF A50-702
India
4450 to IS 202 or 617
International
AlSi7Mg(Fe) to ISO 3522
Japan
AC4C to JIS H5202, AC4C.1 to JIS H2211
Norway
17525 to NS 17525
Russia
AL9 to GOST 2685
South Africa
Al-Si7Mg0.3 to SABS 991, SA14(Al-Si7MgA) to SABS 989
Spain
L-2651 to UNE 38-203, L-2651 to UNE 38-267
UK
LM25 to BS 1490
USA
356, 356 to ASTM B108, 356 to ASTM B26/B26M, 356 to ASTM B618, 356.1, 356.1 to ASTM B179, A03560 to SAE J452, A356.0 to ASTM B26/B26M, A356.0 to MIL A-21180C, UNS A03560, UNS A03561
Tradenames for Aluminum 356.0, Investment Cast, T6
Tradenames
A356
ALLCAST 46
ALLCAST 46A
AS 601
MODULUS METAL Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey