Aluminum, 356.0, investment cast, T6 | Composition

Composition Overview for Aluminum 356.0, Investment Cast, T6 Category Details Compositional Summary Al90-93 / Si6.5-7.5 / Mg0.2-0.45 (impurities: Fe<0.6, Mn<0.35, Zn<0.35, Cu<0.25, Ti<0.25, Other<0.15) Material Family Metal (non-ferrous) Base Material Al (Aluminum) Composition Overview for Aluminum 356.0, Investment Cast, T6 AlSi7Mg(Fe) Composition Overview Composition Detail for Aluminum 356.0, Investment Cast, T6 Element Composition Range Al … Continue reading Aluminum, 356.0, investment cast, T6 | Composition