Mechanical Properties for Aluminum 356.0, Investment Cast, T6
| Property | Value Range |
|---|---|
| Young’s modulus | 71.5 – 74.5 GPa |
| Specific stiffness | 26.6 – 27.8 MN.m/kg |
| Yield strength (elastic limit) | 105 – 116 MPa |
| Tensile strength | 172 – 190 MPa |
| Specific strength | 39 – 43.2 kN.m/kg |
| Elongation | 1 – 1.2 % strain |
| Compressive strength | 105 – 116 MPa |
| Flexural modulus | 71.5 – 74.5 GPa |
| Flexural strength (modulus of rupture) | 110 – 121 MPa |
| Shear modulus | 26.7 – 28.2 GPa |
| Bulk modulus | 66.9 – 76.6 GPa |
| Poisson’s ratio | 0.322 – 0.338 |
| Shape factor | 39 |
| Hardness – Vickers | 89 – 100 HV |
| Elastic stored energy (springs) | 75.3 – 91.8 kJ/m³ |
| Fatigue strength at 10^7 cycles | 74.7 – 91.3 MPa |
| Fatigue strength model (stress range) | 72.2 – 94.4 MPa |
| Mechanical Properties for Aluminum 356.0, Investment Cast, T6 |