Aluminum, 356.0, investment cast, T6 | Equivalent Grades

Standards with Similar Compositions for Aluminum 356.0, Investment Cast, T6 Country/Region Standard/Designation Australia DA601 to AS 1874 Belgium AlSi7 to NBN P21-101 Canada SG70N to CSA HA.10, SG70N to CSA HA.9, SG70P to CSA HA.10, SG70P to CSA HA.9 Czech Republic 424332 to CSN Europe EN AC-42000 to CEN EN 1706 France A-S7G to NF … Continue reading Aluminum, 356.0, investment cast, T6 | Equivalent Grades