Aluminum, 356.0, investment cast, T6 | Mechanical Properties

Mechanical Properties for Aluminum 356.0, Investment Cast, T6 Property Value Range Young’s modulus 71.5 – 74.5 GPa Specific stiffness 26.6 – 27.8 MN.m/kg Yield strength (elastic limit) 105 – 116 MPa Tensile strength 172 – 190 MPa Specific strength 39 – 43.2 kN.m/kg Elongation 1 – 1.2 % strain Compressive strength 105 – 116 MPa … Continue reading Aluminum, 356.0, investment cast, T6 | Mechanical Properties