Aluminum, A356.0, permanent mold cast, F | Mechanical Properties

Aluminum A356.0 permanent mold cast F Mechanical Properties

PropertyValueUnit
Young’s Modulus71.5 – 74.5GPa
Specific Stiffness26.6 – 27.8MN·m/kg
Yield Strength (Elastic Limit)85.5 – 94.5MPa
Tensile Strength170 – 187MPa
Specific Strength31.9 – 35.3kN·m/kg
Elongation2.5 – 3% strain
Compressive Strength 85.5 – 94.5MPa
Flexural Modulus 71.5 – 74.5GPa
Flexural Strength (Modulus of Rupture) 90 – 99MPa
Shear Modulus 26.7 – 28.2GPa
Bulk Modulus 66.9 – 76.6GPa
Poisson’s Ratio0.322 – 0.338—
Shape Factor41—
Hardness – Vickers69 – 77HV
Elastic Stored Energy (Springs)50.1 – 61.1kJ/m³
Fatigue Strength at 10⁷ Cycles100 – 116MPa
Fatigue Strength Model (Stress Range)95.8 – 121MPa
Aluminum A356.0 permanent mold cast F Mechanical Properties

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey