Home » PA (Polyamide / Nylon) » Transparent Polyamide (Transparent Nylon) » Transparent PA Semi-Aromatic Type 6I/6T Amorphous Material Data Sheet
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Material Data Sheet
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Overview
Transparent PA semi-aromatic type 6I/6T amorphous is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Semi-aromatic type 6I/6T, amorphous). This transparent PA semi-aromatic type 6I/6T amorphous material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Designation
Transparent polyamide (nylon) (Semi-aromatic type 6I/6T, amorphous) Tradenames Grivory, Selar, Trogamid, Durethan
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Typical uses
High-voltage switch casings, cable glands, battery seals, keys and push buttons, terminal strips, filter cups, metering devices, inspection glasses, flowmeters, liquid-level indicators, valve blocks, guide rails, coil body, toothbrush handle
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Composition detail
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Physical properties
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Mechanical properties
Young’s modulus 2.94 – 3.66 GPa Specific stiffness 2.49 – 3.1 MN.m/kg Yield strength (elastic limit) 80.1 – 99.9 MPa Tensile strength 101 – 124 MPa Specific strength 67.9 – 84.7 kN.m/kg Elongation 41 – 59 % strain Elongation at yield 3.45 – 6.55 % strain Compressive modulus 3.14 – 3.47 GPa Compressive strength 128 – 142 MPa Flexural modulus 3 – 3.6 GPa Flexural strength (modulus of rupture) 146 – 178 MPa Shear modulus 1.15 – 1.21 GPa Shear strength 60.8 – 74.3 MPa Bulk modulus 5.28 – 5.83 GPa Poisson’s ratio 0.385 – 0.401 Shape factor 4.52 Hardness – Vickers 26 – 28 HV Hardness – Rockwell M 154 – 170 Hardness – Rockwell R 154 – 170 Hardness – Shore D 91 – 95 Hardness – Shore A 97 – 100 Elastic stored energy (springs) 968 – 1540 kJ/m3 Fatigue strength at 10^7 cycles 42.8 – 47.3 MPa Tear strength 159 – 169 N/mm
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Impact & fracture properties
Fracture toughness 3.89 – 4.3 MPa.m0.5 Toughness (G) 4.42 – 5.89 kJ/m2 Impact strength, notched 23 °C 6.8 – 13.2 kJ/m2 Impact strength, notched -30 °C 6.3 – 13.7 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Thermal properties
Glass temperature 120 – 130 °C Heat deflection temperature 0.45MPa 115 °C Heat deflection temperature 1.8MPa 105 °C Vicat softening point 123 – 133 °C Maximum service temperature 40 – 60 °C Minimum service temperature -49 – -29 °C Thermal conductivity 0.206 – 0.214 W/m.°C Specific heat capacity 1400 – 1500 J/kg.°C Thermal expansion coefficient 60 – 80 µstrain/°C Thermal shock resistance 321 – 482 °C Thermal distortion resistance 0.00262 – 0.0035 MW/m
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Electrical properties
Electrical resistivity 2e20 – 5e21 µohm.cm Electrical conductivity 3.45e-20 – 8.62e-19 %IACS Dielectric constant (relative permittivity) 3.82 – 5.38 Dissipation factor (dielectric loss tangent) 0.0264 – 0.0696 Dielectric strength (dielectric breakdown) 20.7 – 35.3 MV/m Comparative tracking index 600 V
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Magnetic properties
Magnetic type Non-magnetic
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Optical, aesthetic and acoustic properties
Refractive index 1.56 – 1.57 Transparency Transparent Acoustic velocity 1580 – 1760 m/s Mechanical loss coefficient (tan delta) 0.0138 – 0.0153
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Absorption & permeability
Water absorption @ 24 hrs 1.2 – 1.9 % Water absorption @ sat 5.2 – 6.8 % Humidity absorption @ sat 1.7 – 2.3 % Water vapor transmission 0.776 – 1.04 g.mm/m².day Permeability (O2) 32 – 42.8 cm³.mm/m².day.atm
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.35 – 0.45 % Melt temperature 260 – 300 °C Mold temperature 60 – 80 °C Molding pressure range 80 – 160 MPa
Transparent PA Semi-Aromatic Type 6I/6T Amorphous Durability
Water (fresh) Acceptable Water (salt) Acceptable Weak acids Limited use Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Unacceptable Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing
Transparent Polyamide Grades
Transparent Polyamide Material Data Sheets
Unfilled Blends with Aliphatic PA, Low Tg Data sheet
Unfilled Cycloaliphatic, Microcrystalline Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, High Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Low Tg Data sheet
Unfilled Part-Cycloaliphatic, Amorphous, Mid Tg Data sheet
Unfilled Semi-Aromatic Type 6-3-T, Amorphous Data sheet
Unfilled Semi-Aromatic Type 6I/6T, Amorphous You are here
Other Transparent Polyamide grades:
All Transparent Polyamide Grades