Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Material Data Sheet

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Material Data Sheet

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Overview

Transparent PA part-cycloaliphatic amorphous mid Tg is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, mid Tg). This transparent PA part-cycloaliphatic amorphous mid Tg material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Designation

Transparent polyamide (nylon) (Part-cycloaliphatic, amorphous, mid Tg)
TradenamesDurethan, Grilamid, Grivory

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Typical uses

Viewing glasses, frames for safety glasses, electrical plugs, IR sensor housing, mobile phone housing, hearing aids, petrol filter, water pressure gauges, sight glasses, sanitary fittings and holders, baby bottles, catering containers, different transparent housings, extruded cable sheathing

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Composition detail

Polymer100  %

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Physical properties

Density1.06–1.08g/cm3

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Mechanical properties

Young’s modulus2.85–3.55GPa
Specific stiffness2.66–3.32MN.m/kg
Yield strength (elastic limit)56.7–70.8MPa
Tensile strength56.7–69.3MPa
Specific strength53–66.2kN.m/kg
Elongation25.9–37.3% strain
Elongation at yield12.2–23.3% strain
Compressive modulus3.04–3.36GPa
Compressive strength71.8–79.4MPa
Flexural modulus2.91–3.49GPa
Flexural strength (modulus of rupture)75.8–92.6MPa
Shear modulus1.11–1.16GPa
Shear strength34–41.6MPa
Bulk modulus5.51–6.09GPa
Poisson’s ratio0.392–0.408 
Shape factor5.32
Hardness – Vickers18–20HV
Hardness – Rockwell M119–131 
Hardness – Rockwell R119–131 
Hardness – Brinell94–117HB
Hardness – Shore D82–86 
Hardness – Shore A90–100 
Elastic stored energy (springs)500–796kJ/m3
Fatigue strength at 10^7 cycles23.9–26.5MPa
Tear strength155–171N/mm

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Impact & fracture properties

Fracture toughness3.87–4.28MPa.m0.5
Toughness (G)4.51–6.02kJ/m2
Impact strength, notched 23 °C7.89–15.3kJ/m2
Impact strength, unnotched 23 °C374–549kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Thermal properties

Glass temperature155–168°C
Heat deflection temperature 0.45MPa135–150°C
Heat deflection temperature 1.8MPa115–136°C
Vicat softening point139–154°C
Maximum service temperature80–100°C
Minimum service temperature-48–-28°C
Thermal conductivity0.099–0.107W/m.°C
Specific heat capacity1710–1780J/kg.°C
Thermal expansion coefficient80–90µstrain/°C
Thermal shock resistance200–276°C
Thermal distortion resistance0.00113–0.0013MW/m

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Electrical properties

Electrical resistivity2e18–5e19µohm.cm
Electrical conductivity3.45e-18–8.62e-17%IACS
Dielectric constant (relative permittivity)3.91–5.51 
Dissipation factor (dielectric loss tangent)0.0207–0.0545 
Dielectric strength (dielectric breakdown)23.2–39.6MV/m
Comparative tracking index600  V

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Magnetic properties

Magnetic typeNon-magnetic

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Optical, aesthetic and acoustic properties

Refractive index1.56–1.58 
TransparencyTransparent
Acoustic velocity1630–1820m/s
Mechanical loss coefficient (tan delta)0.0141–0.0155 

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Absorption & permeability

Water absorption @ 24 hrs0.61–0.99%
Water absorption @ sat2.4–3.2%
Humidity absorption @ sat1.3–1.7%
Water vapor transmission0.776–1.04g.mm/m².day
Permeability (O2)32–42.8cm³.mm/m².day.atm

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.6 – 0.75 %
Melt temperature260 – 290 °C
Mold temperature40 – 120 °C
Molding pressure range34.4 – 138 MPa

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Notes

Transparent PA Part-Cycloaliphatic Amorphous Mid Tg Other notes
Reference grades: Cristamid (Rilsan Clear) 1700, Grilamid TR55, Grilamid TR90