Transparent PA Cycloaliphatic Microcrystalline Material Data Sheet

Transparent PA Cycloaliphatic Microcrystalline Material Data Sheet

Transparent PA Cycloaliphatic Microcrystalline Overview

Transparent PA cycloaliphatic microcrystalline is a grade of transparent polyamide (PA), designated Transparent polyamide (nylon) (cycloaliphatic, microcrystalline). This transparent PA cycloaliphatic microcrystalline material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for transparent polyamide parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined transparent polyamide parts in-house and inspects them before shipment.

Transparent PA Cycloaliphatic Microcrystalline Designation

Transparent polyamide (nylon) (cycloaliphatic, microcrystalline)
TradenamesDurethan, Grilamid, Grivory, Trogamid

Transparent PA Cycloaliphatic Microcrystalline Typical uses

Eyewear frames

Transparent PA Cycloaliphatic Microcrystalline Composition detail

Polymer100  %

Transparent PA Cycloaliphatic Microcrystalline Physical properties

Density0.98–1g/cm3

Transparent PA Cycloaliphatic Microcrystalline Mechanical properties

Young’s modulus1.26–1.58GPa
Specific stiffness1.27–1.6MN.m/kg
Yield strength (elastic limit)45.4–56.6MPa
Tensile strength57.4–70.1MPa
Specific strength45.8–57.2kN.m/kg
Elongation41–59% strain
Elongation at yield5.52–10.5% strain
Compressive modulus1.35–1.49GPa
Compressive strength72.7–80.3MPa
Flexural modulus1.29–1.55GPa
Flexural strength (modulus of rupture)76.8–93.9MPa
Shear modulus0.489–0.514GPa
Shear strength34.4–42.1MPa
Bulk modulus2.68–2.96GPa
Poisson’s ratio0.4–0.416 
Shape factor3.99
Hardness – Vickers15–16HV
Hardness – Rockwell M115–127 
Hardness – Rockwell R115–127 
Hardness – Shore D81–85 
Hardness – Shore A90–100 
Elastic stored energy (springs)721–1150kJ/m3
Fatigue strength at 10^7 cycles24.2–26.8MPa
Tear strength148–164N/mm

Transparent PA Cycloaliphatic Microcrystalline Impact & fracture properties

Fracture toughness3.28–3.63MPa.m0.5
Toughness (G)7.28–9.78kJ/m2
Impact strength, notched 23 °C6.8–13.2kJ/m2
Impact strength, notched -30 °C6.93–15.1kJ/m2
Impact strength, unnotched 23 °C590–600kJ/m2
Impact strength, unnotched -30 °C590–600kJ/m2

Transparent PA Cycloaliphatic Microcrystalline Thermal properties

Melting point224–242°C
Glass temperature132–145°C
Heat deflection temperature 0.45MPa120–126°C
Heat deflection temperature 1.8MPa102–111°C
Vicat softening point125–138°C
Maximum service temperature197–214°C
Minimum service temperature-49–-29°C
Thermal conductivity0.25–0.28W/m.°C
Specific heat capacity1750–1790J/kg.°C
Thermal expansion coefficient88.9–91.1µstrain/°C
Thermal shock resistance342–466°C
Thermal distortion resistance0.00277–0.00312MW/m

Transparent PA Cycloaliphatic Microcrystalline Electrical properties

Electrical resistivity2e18–5e19µohm.cm
Electrical conductivity3.45e-18–8.62e-17%IACS
Dielectric constant (relative permittivity)3.91–5.51 
Dissipation factor (dielectric loss tangent)0.0207–0.0545 
Dielectric strength (dielectric breakdown)24–40.8MV/m
Comparative tracking index600  V

Transparent PA Cycloaliphatic Microcrystalline Magnetic properties

Magnetic typeNon-magnetic

Transparent PA Cycloaliphatic Microcrystalline Optical, aesthetic and acoustic properties

Refractive index1.51–1.52 
TransparencyOptical quality
Acoustic velocity1130–1270m/s
Mechanical loss coefficient (tan delta)0.0211–0.0233 

Transparent PA Cycloaliphatic Microcrystalline Absorption & permeability

Water absorption @ 24 hrs0.59–0.96%
Water absorption @ sat2.6–3.4%
Humidity absorption @ sat0.94–1.3%
Water vapor transmission0.834–0.964g.mm/m².day
Permeability (O2)34.4–39.8cm³.mm/m².day.atm

Transparent PA Cycloaliphatic Microcrystalline Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.4 – 0.8 %
Melt temperature280 – 300 °C
Mold temperature15 – 90 °C
Molding pressure range80 – 160 MPa

Transparent PA Cycloaliphatic Microcrystalline Durability

Water (fresh)Acceptable
Water (salt)Acceptable
Weak acidsLimited use
Strong acidsUnacceptable
Weak alkalisAcceptable
Strong alkalisUnacceptable
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning

Transparent PA Cycloaliphatic Microcrystalline Notes

Transparent PA Cycloaliphatic Microcrystalline Other notes
Reference grades: Rilsan Clear, Trogamid CX 7323