PA612 (Polyamide 612 / Nylon 612)

PA612 (Polyamide 612 / Nylon 612)

PA612 Strengths

PA612 (nylon 612) resists heat better than PA610. Compared with PA6 and PA66 it absorbs less water, keeps its dimensions and electrical properties better and stays tough at lower temperatures. Its mold shrinkage is lower than PA6, PA66 and PA610, and in moist conditions its creep resistance is slightly better than PA66.

PA612 Limitations

Strength and heat distortion temperature are below PA66, and it costs more than PA6 and PA66.

PA612 Designation

PA612, also written 6.12 or 6/12.

Typical Uses of PA612

Mechanical parts, zips, filaments, coverings and coatings that need abrasion resistance.

PA612 Compositional Summary

(NH(CH2)6-NH-CO-(CH2)10-CO)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPA612 (Polyamide / nylon 612)
CAS number26098-55-5

PA612 Processing Properties

Joining

Ultrasonic welding is harder than with PA6 or PA66.

PA612 Parts from Turkey

Looking for PA612 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA612 parts in-house and inspects them before shipment.

PA612 Grades

PA612 Unfilled Grades

PA612 10% PTFE Lubricated Material Data Sheet

PA612 Molding Grade Material Data Sheet

PA612 Toughened Grade Material Data Sheet

PA612 Glass Filled Grades

PA612 30% Glass Fiber Flame Retarded Material Data Sheet

PA612 30-35% Glass Fiber Material Data Sheet

PA612 33% Glass Fiber Toughened Material Data Sheet

PA612 Glass and PTFE Filled Grades

PA612 30% Glass Fiber 15% PTFE Lubricated Material Data Sheet

PA612 Carbon and PTFE Filled Grades

PA612 30% Carbon Fiber 10% PTFE Lubricated Material Data Sheet