PEK (polyetherketone) is a high-temperature semi-crystalline thermoplastic of the polyether ketone family.
PEK Strengths
PEK has higher melting and glass transition temperatures than PEEK, though lower than PEKK, and slightly better stiffness and tensile strength than PEEK.
PEK Limitations
It costs more than PEEK and needs even higher mold temperatures than PEEK, which are already high.
PEK Designation
Chemical name: poly(oxy-1,4-phenylenecarbonyl-1,4-phenylene). Tradenames include Ultrapek, Luvocom and PEEK-HT.
Typical Uses of PEK
Bearing cages, gear support bearings, thrust washers, clutch seals, transmission parts, tire pressure sensor housings, valve spring discs, rollers, guides, gears and reciprocating components.
PEK Compositional Summary
(-C6H4-O-C6H4-(C=O)-)n
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PEK (Polyetherketone)
CAS number
27380-27-4
Effect of Composition on PEK
A higher share of ketone groups (33% in PEEK, 50% in PEK, 67% in PEKK) raises the melting and glass transition temperatures. Other properties change little, apart from a small gain in stiffness and tensile strength.
PEK Processing Properties
First Commercial Production
1986
Forming
PEK can be compression molded, injection molded, extruded and vacuum formed. It needs very high melt temperatures, and pre-drying is essential because of the high mold temperatures. Fine powder can coat metal parts up to about 2 mm thick by vortex sintering.
Machining
The material machines very easily. Carbide or diamond-tipped tools with water cooling are recommended, and the parts should be annealed before machining.
Joining
Solvent bonding is difficult, but a wide range of adhesives works well, and surface treatment such as laser treatment greatly improves bond strength. All welding methods except radio-frequency welding are suitable, although hot gas welding is difficult and the high melting point means welding needs a lot of energy. Laser welding works, the material can be welded to PEI, and welds to aluminum have had some success. Films can be heat sealed at high temperatures.