PEEK 10% Glass Fiber Material Data Sheet

PEEK 10% Glass Fiber (Polyetheretherketone) Material Data Sheet

PEEK 10% Glass Fiber Overview

PEEK 10% glass fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (10% Glass Fiber). This PEEK 10% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

PEEK Designation

Polyetheretherketone (10% Glass Fiber)
TradenamesEdgetek, Hifill, Instruc, LNP Thermocomp, RTP

PEEK Typical uses

Aerospace applications, automotive applications, consumer applications, general purpose, industrial applications, structural parts

PEEK 10% Glass Fiber Composition detail

Polymer90  %
Glass (fiber)10  %

PEEK Physical properties

Density1.37–1.39g/cm3

PEEK 10% Glass Fiber Mechanical properties

Young’s modulus5.52–6.5GPa
Specific stiffness4–4.71MN.m/kg
Yield strength (elastic limit)103–120MPa
Tensile strength107–125MPa
Specific strength74.6–87kN.m/kg
Elongation4–4.5% strain
Elongation at yield2.44–4.14% strain
Compressive modulus3.51–3.68GPa
Compressive strength129–142MPa
Flexural modulus5.17–6.01GPa
Flexural strength (modulus of rupture)153–203MPa
Shear modulus2.09–2.19GPa
Shear strength64.6–71.2MPa
Bulk modulus5.52–6.5GPa
Poisson’s ratio0.39–0.41 
Shape factor5.5
Hardness – Vickers27–29HV
Hardness – Rockwell R118–124 
Hardness – Shore D89–96 
Elastic stored energy (springs)874–1220kJ/m3
Fatigue strength at 10^7 cycles41.1–49.7MPa

PEEK Impact & fracture properties

Fracture toughness6.12–8.81MPa.m0.5
Toughness (G)6.39–12.7kJ/m2
Impact strength, notched 23 °C4.6–8.5kJ/m2
Impact strength, unnotched 23 °C39.4–85.6kJ/m2

PEEK 10% Glass Fiber Thermal properties

Melting point343  °C
Glass temperature306–318°C
Heat deflection temperature 0.45MPa285–326°C
Heat deflection temperature 1.8MPa170–235°C
Maximum service temperature220–250°C
Thermal conductivity0.3  W/m.°C
Specific heat capacity1390–1450J/kg.°C
Thermal expansion coefficient29–44µstrain/°C
Thermal shock resistance413–654°C
Thermal distortion resistance0.00682–0.0103MW/m

PEEK Electrical properties

Electrical resistivity10000000000000000000000  µohm.cm
Electrical conductivity1.72e-20 %IACS
Dielectric constant (relative permittivity)3.1
Dielectric strength (dielectric breakdown)18  MV/m

PEEK Magnetic properties

Magnetic typeNon-magnetic

PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2000–2170m/s
Mechanical loss coefficient (tan delta)0.009–0.013 

PEEK Absorption & permeability

Water absorption @ 24 hrs0.102–0.32%
Humidity absorption @ sat0.12  %

PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.3 – 0.8 %
Melt temperature349 – 399 °C
Mold temperature149 – 218 °C
Molding pressure range82.7 – 124 MPa

PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing