Home » PEEK (Polyetheretherketone) » Modified PEEK 25-30% Carbon Wear Grade Material Data Sheet
Modified PEEK 25-30% Carbon Wear Grade (Polyetheretherketone) Material Data Sheet
Modified PEEK 25-30% Carbon Wear Grade Overview
Modified PEEK 25-30% carbon wear grade is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (Wear grade). This modified PEEK 25-30% carbon wear grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
Modified PEEK Designation
Modified poly(etheretherketone) (Wear grade) Tradenames AvaSpire
Modified PEEK 25-30% Carbon Wear Grade Composition detail
Polymer 65 – 75 % PTFE (lubricant) 0 – 10 % Carbon (fiber) 15 – 25 % Graphite (powder) 0 – 10 %
Modified PEEK Physical properties
Modified PEEK 25-30% Carbon Wear Grade Mechanical properties
Young’s modulus 12.3 – 13.1 GPa Specific stiffness 8.37 – 8.97 MN.m/kg Yield strength (elastic limit) 111 – 118 MPa Tensile strength 135 – 144 MPa Specific strength 75.7 – 80.7 kN.m/kg Elongation 1.74 – 2.16 % strain Elongation at yield 1.7 – 2.1 % strain Compressive modulus 12.3 – 13.1 GPa Flexural modulus 12.3 – 13.1 GPa Flexural strength (modulus of rupture) 211 – 213 MPa Shear modulus 4.6 – 4.9 GPa Shear strength 67.5 – 74.5 MPa Poisson’s ratio 0.42 – 0.46 Shape factor 8.8 Hardness – Vickers 33 – 35 HV Elastic stored energy (springs) 482 – 552 kJ/m3 Fatigue strength at 10^7 cycles 53 – 58.6 MPa
Modified PEEK Impact & fracture properties
Impact strength, notched 23 °C 4.97 – 7.23 kJ/m2 Impact strength, unnotched 23 °C 40.2 – 45.8 kJ/m2
Modified PEEK 25-30% Carbon Wear Grade Thermal properties
Melting point 613 – 616 °C Glass temperature 150 – 168 °C Heat deflection temperature 0.45MPa 554 – 563 °C Heat deflection temperature 1.8MPa 540 – 549 °C Vicat softening point 554 – 563 °C Thermal conductivity 0.3 – 0.34 W/m.°C Specific heat capacity 1350 – 1380 J/kg.°C Thermal expansion coefficient 9.88 – 10.1 µstrain/°C Thermal shock resistance 862 – 945 °C Thermal distortion resistance 0.03 – 0.0341 MW/m
Modified PEEK Electrical properties
Electrical resistivity 25000000000000000 – 100000000000000000 µohm.cm Electrical conductivity 1.72e-15 – 6.9e-15 %IACS Dielectric constant (relative permittivity) 3.3 – 4 Dissipation factor (dielectric loss tangent) 0.001 – 0.006 Dielectric strength (dielectric breakdown) 30 – 70 MV/m Galvanic potential 0.14 – 0.22 V
Modified PEEK Magnetic properties
Magnetic type Non-magnetic
Modified PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2890 – 3000 m/s
Modified PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Acceptable Polymer thermoforming Unsuitable Melt temperature 366 – 388 °C Mold temperature 149 – 177 °C
Modified PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
Modified PEEK Carbon Filled Material Data Sheets
All PEEK Grades
Modulus Metal Services