Home » PEEK (Polyetheretherketone) » PEEK 30% Carbon Fiber Material Data Sheet
PEEK 30% Carbon Fiber (Polyetheretherketone) Material Data Sheet
PEEK 30% Carbon Fiber Overview
PEEK 30% carbon fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (30% Carbon Fiber). This PEEK 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (30% Carbon Fiber) Tradenames Gatone, Kebapeak, Ketaspire, Ketron, Larpeek, LNP Thermocomp, Luvocom, Schulatec, Vestakeep, Victrex
PEEK Typical uses
Wire covering, injection molded engineering products, film for flexible pcb, resin in fiber prepegs, aerospace applications, radiation environments, piping.
PEEK 30% Carbon Fiber Composition detail
Polymer 70 % Carbon (fiber) 30 %
PEEK Physical properties
PEEK 30% Carbon Fiber Mechanical properties
Young’s modulus 20.7 – 25 GPa Specific stiffness 14.5 – 17.5 MN.m/kg Yield strength (elastic limit) 190 – 228 MPa Tensile strength 190 – 228 MPa Specific strength 133 – 159 kN.m/kg Elongation 1 – 4 % strain Compressive modulus 12.4 – 15 GPa Compressive strength 172 – 240 MPa Flexural modulus 17.2 – 23 GPa Flexural strength (modulus of rupture) 276 – 335 MPa Shear modulus 7.3 – 8.8 GPa Bulk modulus 25.9 – 31.3 GPa Poisson’s ratio 0.43 – 0.45 Shape factor 8.7 Hardness – Vickers 49 – 55 HV Hardness – Rockwell M 100 – 110 Hardness – Rockwell R 121 – 127 Elastic stored energy (springs) 784 – 1160 kJ/m3 Fatigue strength at 10^7 cycles 115 – 127 MPa
PEEK Impact & fracture properties
Fracture toughness 6.34 – 7.89 MPa.m0.5 Toughness (G) 1.76 – 2.75 kJ/m2 Impact strength, notched 23 °C 8.18 – 9.9 kJ/m2 Impact strength, notched -30 °C 7.27 – 8.8 kJ/m2 Impact strength, unnotched 23 °C 50 – 60.5 kJ/m2 Impact strength, unnotched -30 °C 50 – 60.5 kJ/m2
PEEK 30% Carbon Fiber Thermal properties
Melting point 322 – 346 °C Glass temperature 143 – 157 °C Heat deflection temperature 0.45MPa 295 – 354 °C Heat deflection temperature 1.8MPa 288 – 321 °C Maximum service temperature 260 – 280 °C Minimum service temperature -70 – -50 °C Thermal conductivity 0.87 – 0.97 W/m.°C Specific heat capacity 1360 – 1410 J/kg.°C Thermal expansion coefficient 10 – 15 µstrain/°C Thermal shock resistance 591 – 944 °C Thermal distortion resistance 0.0609 – 0.0924 MW/m
PEEK Electrical properties
Electrical resistivity 1000000 – 10000000 µohm.cm Electrical conductivity 1.72e-5 – 1.72e-4 %IACS Galvanic potential 0.14 – 0.22 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3800 – 4190 m/s Mechanical loss coefficient (tan delta) 0.00431 – 0.00671
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.06 – 0.12 %
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.05 – 1.4 % Melt temperature 309 – 427 °C Mold temperature 120 – 160 °C Molding pressure range 68.8 – 138 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
Modulus Metal Services
Manufacturing & Quality Services in Turkey