Home » PEEK (Polyetheretherketone) » Modified PEEK Unfilled Grade Material Data Sheet
Modified PEEK Unfilled Grade (Polyetheretherketone) Material Data Sheet
Modified PEEK Unfilled Grade Overview
Modified PEEK unfilled grade is a grade of polyetheretherketone (PEEK), designated Modified poly(etheretherketone) (unfilled). This modified PEEK unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
Modified PEEK Designation
Modified poly(etheretherketone) (unfilled) Tradenames Latigray, Latiohm, LNP Lubricomp, LNP Stat-Kon, LNP Thermocomp, Lubricomp, Optestat, Thermocomp
Modified PEEK Unfilled Grade Composition detail
Modified PEEK Physical properties
Modified PEEK Unfilled Grade Mechanical properties
Young’s modulus 2.69 – 3.51 GPa Specific stiffness 2.07 – 2.7 MN.m/kg Yield strength (elastic limit) 70 – 75 MPa Tensile strength 81.8 – 88.8 MPa Specific strength 53.8 – 57.8 kN.m/kg Elongation 28.8 – 43.8 % strain Elongation at yield 5.28 – 6.52 % strain Compressive modulus 2.69 – 3.51 GPa Flexural modulus 2.8 – 3.55 GPa Flexural strength (modulus of rupture) 117 – 136 MPa Shear modulus 1 – 1.3 GPa Shear strength 75.5 – 83.5 MPa Poisson’s ratio 0.39 – 0.43 Shape factor 4.9 Hardness – Vickers 21 – 22 HV Elastic stored energy (springs) 738 – 989 kJ/m3 Fatigue strength at 10^7 cycles 32.4 – 35.8 MPa
Modified PEEK Impact & fracture properties
Impact strength, notched 23 °C 7.16 – 9.84 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2
Modified PEEK Unfilled Grade Thermal properties
Melting point 613 – 618 °C Glass temperature 149 – 167 °C Heat deflection temperature 0.45MPa 445 – 538 °C Heat deflection temperature 1.8MPa 434 – 525 °C Vicat softening point 445 – 538 °C Thermal conductivity 0.2 – 0.24 W/m.°C Specific heat capacity 1520 – 1560 J/kg.°C Thermal expansion coefficient 45 – 47 µstrain/°C Thermal shock resistance 447 – 588 °C Thermal distortion resistance 0.00434 – 0.00523 MW/m
Modified PEEK Electrical properties
Electrical resistivity 25000000000000000 – 100000000000000000 µohm.cm Electrical conductivity 1.72e-15 – 6.9e-15 %IACS Dielectric constant (relative permittivity) 3.3 – 4 Dissipation factor (dielectric loss tangent) 0.001 – 0.006 Dielectric strength (dielectric breakdown) 30 – 70 MV/m
Modified PEEK Magnetic properties
Magnetic type Non-magnetic
Modified PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1440 – 1650 m/s
Modified PEEK Absorption & permeability
Water absorption @ 24 hrs 0.1 – 0.2 % Water absorption @ sat 0.45 – 0.55 %
Modified PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Acceptable Polymer thermoforming Unsuitable Linear mold shrinkage 1.1 – 1.5 % Melt temperature 366 – 388 °C Mold temperature 149 – 204 °C
Modified PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oils and fuels Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
Modified PEEK Unfilled Material Data Sheets
Unfilled Unfilled You are here
All PEEK Grades