Home » PEEK (Polyetheretherketone) » PEEK Unfilled Grade Material Data Sheet
PEEK Unfilled Grade (Polyetheretherketone) Material Data Sheet
PEEK Unfilled Grade Overview
PEEK unfilled grade is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (Unfilled). This PEEK unfilled grade material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.
PEEK Designation
Polyetheretherketone (Unfilled) Tradenames Aptiv, Chemerize, Dynamix, Gatone, Hifill, Ketaspire, Ketron, Larpeek, Luvocom, Meldin, Nemcon, Peek-Optima, Schulatec, Tecapeek, Vestakeep, Vicote, Victrex
PEEK Typical uses
Wire covering, injection molded engineering products, film for flexible pcb, resin in fiber prepegs, aerospace applications, radiation environments, medical devices.
PEEK Unfilled Grade Composition detail
PEEK Physical properties
PEEK Unfilled Grade Mechanical properties
Young’s modulus 3.76 – 3.95 GPa Specific stiffness 2.87 – 3.02 MN.m/kg Yield strength (elastic limit) 87 – 95 MPa Tensile strength 70.3 – 103 MPa Specific strength 66.4 – 72.6 kN.m/kg Elongation 30 – 150 % strain Compressive modulus 3.76 – 3.95 GPa Compressive strength 118 – 130 MPa Flexural modulus 3.76 – 3.95 GPa Flexural strength (modulus of rupture) 105 – 116 MPa Shear modulus 1.36 – 1.43 GPa Bulk modulus 5.48 – 5.75 GPa Poisson’s ratio 0.39 – 0.41 Shape factor 4.9 Hardness – Vickers 26 – 29 HV Hardness – Rockwell M 95 – 105 Hardness – Rockwell R 119 – 131 Elastic stored energy (springs) 981 – 1170 kJ/m3 Fatigue strength at 10^7 cycles 28.1 – 41.2 MPa
PEEK Impact & fracture properties
Fracture toughness 2.73 – 4.3 MPa.m0.5 Toughness (G) 2.02 – 4.6 kJ/m2 Impact strength, notched 23 °C 5.91 – 7.15 kJ/m2 Impact strength, notched -30 °C 5.91 – 7.15 kJ/m2 Impact strength, unnotched 23 °C 590 – 600 kJ/m2 Impact strength, unnotched -30 °C 590 – 600 kJ/m2
PEEK Unfilled Grade Thermal properties
Melting point 322 – 346 °C Glass temperature 143 – 157 °C Heat deflection temperature 0.45MPa 164 – 208 °C Heat deflection temperature 1.8MPa 139 – 182 °C Maximum service temperature 239 – 260 °C Minimum service temperature -70 – -50 °C Thermal conductivity 0.24 – 0.26 W/m.°C Specific heat capacity 1340 J/kg.°C Thermal expansion coefficient 50 – 60 µstrain/°C Thermal shock resistance 389 – 477 °C Thermal distortion resistance 0.00413 – 0.00503 MW/m
PEEK Electrical properties
Electrical resistivity 3300000000000000000000 – 30000000000000000000000 µohm.cm Electrical conductivity 5.75e-21 – 5.22e-20 %IACS Dielectric constant (relative permittivity) 3.1 – 3.3 Dissipation factor (dielectric loss tangent) 0.0015 – 0.0017 Dielectric strength (dielectric breakdown) 16.7 – 20 MV/m Comparative tracking index 175 – 225 V
PEEK Magnetic properties
Magnetic type Non-magnetic
PEEK Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1690 – 1740 m/s Mechanical loss coefficient (tan delta) 0.0101 – 0.0106
PEEK Absorption & permeability
Water absorption @ 24 hrs 0.1 – 0.14 % Permeability (O2) 6.54 – 11.3 cm³.mm/m².day.atm
PEEK Processing properties
Polymer injection molding Limited use Polymer extrusion Acceptable Polymer thermoforming Limited use Linear mold shrinkage 1 – 1.21 % Melt temperature 349 – 399 °C Mold temperature 120 – 160 °C Molding pressure range 68.8 – 138 MPa
PEEK Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Excellent Flammability Self-extinguishing
PEEK Grades
PEEK Unfilled Material Data Sheets
Unfilled Unfilled You are here
All PEEK Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey