PEEK 15% Glass Fiber Material Data Sheet

PEEK 15% Glass Fiber (Polyetheretherketone) Material Data Sheet

PEEK 15% Glass Fiber Overview

PEEK 15% glass fiber is a grade of polyetheretherketone (PEEK), designated Polyetheretherketone (15% Glass Fiber). This PEEK 15% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PEEK parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PEEK parts in-house and inspects them before shipment.

PEEK Designation

Polyetheretherketone (15% Glass Fiber)
TradenamesKetaspire, Larpeek, LNP Thermocomp, Luvocom, RTP, Vampeek, Victrex

PEEK Typical uses

Aerospace applications, automotive applications, connectors, dental applications, electrical/electronic applications, film, food applications (non-specific), hospital goods, industrial applications, medical appliances, oil/gas applications, parts (engineering), pump parts, seals, surgical instruments, textile applications

PEEK 15% Glass Fiber Composition detail

Polymer85  %
Glass (fiber)15  %

PEEK Physical properties

Density1.38–1.41g/cm3

PEEK 15% Glass Fiber Mechanical properties

Young’s modulus6.38–7.56GPa
Specific stiffness4.57–5.43MN.m/kg
Yield strength (elastic limit)110–137MPa
Tensile strength117–140MPa
Specific strength78.8–98.3kN.m/kg
Elongation2.32–4.8% strain
Elongation at yield2–3.9% strain
Compressive modulus4.07–4.27GPa
Compressive strength200  MPa
Flexural modulus5.6–7.5GPa
Flexural strength (modulus of rupture)193–240MPa
Shear modulus2.42–2.54GPa
Shear strength73.1–80.6MPa
Bulk modulus6.38–7.56GPa
Poisson’s ratio0.39–0.41 
Shape factor5.7
Hardness – Vickers30–32HV
Hardness – Shore D86
Elastic stored energy (springs)869–1350kJ/m3
Fatigue strength at 10^7 cycles46.5–56.3MPa

PEEK Impact & fracture properties

Fracture toughness6.39–9.2MPa.m0.5
Toughness (G)6–11.9kJ/m2
Impact strength, notched 23 °C4.82–9.1kJ/m2
Impact strength, notched -30 °C3  kJ/m2
Impact strength, unnotched 23 °C45–91kJ/m2
Impact strength, unnotched -30 °C40  kJ/m2

PEEK 15% Glass Fiber Thermal properties

Melting point343  °C
Glass temperature143  °C
Heat deflection temperature 0.45MPa290–329°C
Heat deflection temperature 1.8MPa216–321°C
Vicat softening point300–335°C
Maximum service temperature220–250°C
Thermal conductivity0.3  W/m.°C
Specific heat capacity1700  J/kg.°C
Thermal expansion coefficient25–50µstrain/°C
Thermal shock resistance347–719°C
Thermal distortion resistance0.006–0.012MW/m

PEEK Electrical properties

Electrical resistivity1000000000000000000000–10000000000000000000000µohm.cm
Electrical conductivity1.72e-20–1.72e-19%IACS
Dielectric constant (relative permittivity)3.1
Dielectric strength (dielectric breakdown)23–24MV/m
Comparative tracking index150–200V

PEEK Magnetic properties

Magnetic typeNon-magnetic

PEEK Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2140–2330m/s
Mechanical loss coefficient (tan delta)0.0084–0.012 

PEEK Absorption & permeability

Water absorption @ 24 hrs0.06–0.17%
Humidity absorption @ sat0.4  %

PEEK Processing properties

Polymer injection moldingLimited use
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.3 – 0.9 %
Melt temperature349 – 400 °C
Mold temperature149 – 218 °C
Molding pressure range68.9 – 124 MPa

PEEK Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsUnacceptable
Weak alkalisExcellent
Strong alkalisExcellent
Organic solventsExcellent
Oxidation at 500CUnacceptable
UV radiation (sunlight)Excellent
FlammabilitySelf-extinguishing