15-5PH H1150M Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
15-5PH H1150M Stainless Steel Overview
15-5PH H1150M stainless steel is a martensitic precipitation hardening stainless steel (UNS S15500) in the wrought form. Condition: H1150M (Solution annealed; precipitation (age) hardened at 760°C; air cooled). This 15-5PH H1150M stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for 15-5PH parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined 15-5PH parts in-house and inspects them before shipment.
15-5PH Designation
15-5PH, wrought
Condition
H1150M (Solution annealed; precipitation (age) hardened at 760°C; air cooled)
UNS number
S15500
US name
15-5PH
15-5PH Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide
Susceptible
Intergranular (weld line) corrosion
Good
Inorganic acids
Restricted
Organic acids
Moderate
Alkalis
Moderate
Humidity / water
Excellent
Sea water
Restricted
Sour oil and gas
Restricted
15-5PH Standards with similar compositions
China: 0Cr16Ni4Cu4Nb to GB 8732
France: Z6CNU15.05 to AFNOR NF A35-581
Germany: GX4CrNiCuNb16-4 to DIN
USA: 17-4PH to SAE J467, 5658 to AMS 5658, 5659 to AMS 5659, 5826 to AMS 5826, 5862 to AMS 5862, S15500 to ASTM A564/A564M, S15500 to ASTM A693, S15500 to ASTM A705/A705M-95, S15500 to ASTM A959, UNS J92110, UNS S15500