PH 13-8Mo H1100 Stainless Steel Material Data Sheet
PH 13-8Mo H1100 Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
PH 13-8Mo H1100 Stainless Steel Overview
PH 13-8Mo H1100 stainless steel is a martensitic precipitation hardening stainless steel (UNS S13800) in the wrought form. Condition: H1100 (Solution annealed; precipitation (age) hardened at 593°C; air cooled). This PH 13-8Mo H1100 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for PH 13-8Mo parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PH 13-8Mo parts in-house and inspects them before shipment.
PH 13-8Mo Designation
Korloy 2573, wrought
Condition
H1100 (Solution annealed; precipitation (age) hardened at 593°C; air cooled)
UNS number
S13800
US name
PH 13-8Mo
EN name
X3CrNiMoAl13-8-2
EN number
1.4534
PH 13-8Mo Typical uses
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes