17-4PH H1150M Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
17-4PH H1150M Stainless Steel Overview
17-4PH H1150M stainless steel is a martensitic precipitation hardening stainless steel (UNS S17400) in the wrought form. Condition: H1150M (Solution annealed; precipitation (age) hardened at 760°C; air cooled). This 17-4PH H1150M stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for 17-4PH parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined 17-4PH parts in-house and inspects them before shipment.
17-4PH Designation
17-4PH, wrought
Condition
H1150M (Solution annealed; precipitation (age) hardened at 760°C; air cooled)
Processing of potentially corrosive liquids e.g. chemicals/oil/beverages/sewage, structural uses in corrosive environments, e.g. nuclear plants, ships, offshore oil installations, underwater cables and pipes
Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide
Susceptible
Intergranular (weld line) corrosion
Good
Inorganic acids
Restricted
Organic acids
Moderate
Alkalis
Moderate
Humidity / water
Excellent
Sea water
Restricted
Sour oil and gas
Restricted
17-4PH Standards with similar compositions
Australia: 630 to AS 2837
China: 0Cr17Ni4Cu4Nb to GB 1220, 0Cr17Ni4Cu4Nb to GB 1221
France: Z4CNU17.4M to AFNOR NF A35-586, Z6CNU17.04 to AFNOR NF A35-581
Germany: 1.4542 to DIN EN 10088, X5CrNiCuNb16-4 to DIN EN 10088
Japan: SUS630 to JIS G4303, SUS630 to JIS G4304, SUS630 to JIS G4305, SUS630FB to JIS G4319, SUSF630 to JIS G3214
South Korea: STS 630 to KS D 3706, STS F 630 to KS D 4115, STS630 to KS D 3698, STS630 to KS D 3705, STS630FB to KS D 3691
USA: 17-4 PH to MIL-C-24111B, 5604 to AMS 5604, 5622 to AMS 5622, 5643 to AMS 5643P, 61 to ASTM A579, Grade F Class 1 to ASTM A1028, Grade F Class 1 to ASTM A982, IC-17-4 to MIL-S-81591, S17400 to ASTM A564/A564M, S17400 to ASTM A693, S17400 to ASTM A705/A705M-95, S17400 to ASTM A959, S17400 to ASTM F594, S17400 to ASTM F738M, S17400 to ASTM F836M, UNS S17400