AISI 1015 Equivalent Grades-Similar Compositions

AISI 1015 Similar Compositions

China: ML15Al to GB/T 6478
India: 12C5 to IS 8053, 14C4 to IS 1871/2, 14C6 to IS 11169/1, 14C6 to IS 1570/2/1, C14 to IS 1570/2/1, C15Mn75 to IS 6967, CDS-2 to IS 3074, Fe 310 to IS 12367, Grade 6 to IS 7887, Grade 6 to IS 8952, Grade 7 to IS 7887, Grade 7 to IS 8952
International: CC15A to ISO 4954, CC15X to ISO 4954
Japan: SGD 3 to JIS G3108, SWRCH15A to JIS G3507, SWRCH15R to JIS G3507, SWRCH17R to JIS G3507, SWRM 15 to JIS G3505, SWRM 17 to JIS G3505
Mexico: 1015 to NMX-B-301, 1017 to NMX-B-301, MT1015 to NMX-B-201, MT1015 to NMX-B-203-SCFI
Pan America: 1015 to COPANT 330, 1015 to COPANT 331, 1015 to COPANT 333, 1017 to COPANT 333
South Korea: SGD 3 to KS D 3526, SWRCH15A to KS D 3592, SWRCH15R to KS D 3592, SWRCH17R to KS D 3592, SWRM 15 to KS D 3554, SWRM 17 to KS D 3554
Spain: 16KA-DF to UNE 36032, F.7515 to UNE 36032
UK: 040A17 to BS 970/1, HS17 to BS 1449 Section 1.14
USA: 1013 to SAE J403, 1015, 1015 to ASTM A29/A29M, 1015 to ASTM A512-96, 1015 to ASTM A513, 1015 to ASTM A519, 1015 to ASTM A568/A568M, 1015 to ASTM A787, 1015 to DoD-F-24669/1, 1015 to FED QQ-S-698, 1015 to FED QQ-W-461H, 1015 to MIL-T-3520, 1015 to SAE J403, 1017, 1017 to ASTM A29/A29M, 1017 to ASTM A513, 1017 to ASTM A519, 1017 to ASTM A568/A568M, 1017 to ASTM A787, 1017 to SAE J403, 5061 to AMS 5061E, G10150 to ASTM A510/A510M, G10150 to ASTM A576-90b, G10150 to ASTM A830/A830M, G10170 to ASTM A510/A510M, G10170 to ASTM A576-90b, G10170 to ASTM A830/A830M, Grade B to ASTM A31, Grade C to ASTM A1020/A1020M, Grade C to ASTM A178/A178M, Grade C to ASTM A285/A285M, M1015, M1015 to ASTM A29/A29M, M1015 to ASTM A575-96, M1015 to SAE J403, M1017, M1017 to ASTM A29/A29M, M1017 to ASTM A575-96, MT1015 to ASTM A512-96, MT1015 to ASTM A513, MT1015 to ASTM A519, MT1015 to ASTM A787, UNS G10150, UNS G10150 to UNS, UNS G10170, UNS G10170 to UNS, UNS K00802, UNS K01602, UNS K02801, UNS K03003, UNS K03007, UNS K03100, UNS K03503

General information

Designation: AISI 1015
UNS numberG10150
US nameASTM MT1015, ASTM M1015, ASTM G10170, ASTM 1015, ASME G10150, ~SAE SAE J525, ~SAE SAE J524, ~SAE SAE J356, ~ASTM A822, ~ASTM A214, ~ASTM A2
EN nameHS17, ~UkSt37-2, ~P235T1, ~C15R, ~C15E, ~C15
EN number~1.1141, ~1.1140, ~1.0124
ISO name~R33, ~CE15E4, ~CC15X, ~CC15A
GB (Chinese) name~ML15Al, ~CRB650
JIS (Japanese) nameSWRM 17, SWRM 15, SWRCH17R, SWRCH15R, SGD 3, ~SWRCH15A

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey