AISI 1015 Carbon Steel General Information

General information Designation: AISI 1015 UNS number G10150 US name ASTM MT1015, ASTM M1015, ASTM G10170, ASTM 1015, ASME G10150, ~SAE SAE J525, ~SAE SAE J524, ~SAE SAE J356, ~ASTM A822, ~ASTM A214, ~ASTM A2 EN name HS17, ~UkSt37-2, ~P235T1, ~C15R, ~C15E, ~C15 EN number ~1.1141, ~1.1140, ~1.0124 ISO name ~R33, ~CE15E4, ~CC15X, ~CC15A GB … Continue reading AISI 1015 Carbon Steel General Information