AISI 1015 Carbon Steel Chemical Composition

AISI 1015 Composition detail

C (carbon)0.130.18%
Fe (iron)99.199.6%
Mn (manganese)0.30.6%
P (phosphorus)00.04%
S (sulfur)00.05%

Designation: AISI 1015
UNS numberG10150
US nameASTM MT1015, ASTM M1015, ASTM G10170, ASTM 1015, ASME G10150, ~SAE SAE J525, ~SAE SAE J524, ~SAE SAE J356, ~ASTM A822, ~ASTM A214, ~ASTM A2
EN nameHS17, ~UkSt37-2, ~P235T1, ~C15R, ~C15E, ~C15
EN number~1.1141, ~1.1140, ~1.0124
ISO name~R33, ~CE15E4, ~CC15X, ~CC15A
GB (Chinese) name~ML15Al, ~CRB650
JIS (Japanese) nameSWRM 17, SWRM 15, SWRCH17R, SWRCH15R, SGD 3, ~SWRCH15A

MODULUS METAL
Sand Casting in TurkeyPermanent Mold Casting in TurkeyGravity Die Casting in TurkeyPressure Die Casting in TurkeyHigh-Pressure Die Casting in TurkeyInvestment Casting in TurkeyFoundry in TurkeyPlastic Injection Molding in TurkeyPress Bending ( Press Brake) Products in TurkeyLaser and Plasma Cutting in TurkeyWelded Construction in Turkey, Heat TreatedCNC Machined Products Manufacturer in TurkeyAdditive Manufacturing and 3D Printing in TurkeyQuality Enginering and Inspection Service in TurkeyManufacturing Inspection Service in TurkeyQuality Engineering and Supplier Quality Engineering Service in TurkeySupplier Quality Control and Inspection Service in TurkeyResident Engineering Services in Turkey