AISI 1015 Normalized Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 300 – 355 MPa Tensile strength 380 – 470 MPa Specific strength 38.2 – 45.2 kN.m/kg Elongation 29 – 45 % strain Compressive strength 300 – 355 MPa Flexural modulus 205 – 215 GPa … Continue reading AISI 1015 Normalized Carbon Steel Mechanical Properties