AISI 1015 As Rolled Carbon Steel Mechanical Properties
AISI 1015 As rolled Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 280 – 345 MPa Tensile strength 375 – 465 MPa Specific strength 35.7 – 44 kN.m/kg Elongation 31 – 47 % strain Compressive strength 280 – 345 MPa Flexural modulus 205 – 215 … Continue reading AISI 1015 As Rolled Carbon Steel Mechanical Properties