AISI 1015 Carbon Steel Chemical Composition
AISI 1015 Composition detail C (carbon) 0.13 – 0.18 % Fe (iron) 99.1 – 99.6 % Mn (manganese) 0.3 – 0.6 % P (phosphorus) 0 – 0.04 % S (sulfur) 0 – 0.05 % Designation: AISI 1015 UNS number G10150 US name ASTM MT1015, ASTM M1015, ASTM G10170, ASTM 1015, ASME G10150, ~SAE SAE J525, … Continue reading AISI 1015 Carbon Steel Chemical Composition