Aluminum 6005A T5 Mechanical Properties

Designation: Aluminum 6005A T5

6005A, wrought
ConditionT5 (Cooled from an elevated-temperature shaping process and artificially aged)
UNS numberA96005A
EN nameEN AW-6005A
EN number3.3210
ISO nameAl SiMg(A)
JIS (Japanese) nameA6NO1

Mechanical properties: Aluminum 6005A T5

Young’s modulus67.5–71GPa
Specific stiffness24.9–26.3MN.m/kg
Yield strength (elastic limit)200–233MPa
Tensile strength255–297MPa
Specific strength73.9–86.2kN.m/kg
Elongation8–11.5% strain
Compressive strength208–243MPa
Flexural modulus67.5–71GPa
Flexural strength (modulus of rupture)208–243MPa
Shear modulus27–28.4GPa
Bulk modulus67.5–71GPa
Poisson’s ratio0.325–0.335 
Shape factor28.7   
Hardness – Vickers95–100HV
Elastic stored energy (springs)290–391kJ/m^3
Fatigue strength at 10^7 cycles93.5–109MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles85.6–119MPa

Impact & fracture properties: Aluminum 6005A T5

Fracture toughness30–36MPa.m^0.5
Toughness (G)13.1–18.6kJ/m^2

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey