AISI 1030 As Rolled Material Data Sheet
AISI 1030 As Rolled Overview
| AISI 1030 as rolled is AISI 1030 medium carbon steel (UNS G10300) in the as rolled condition. This AISI 1030 as rolled material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Compare all AISI 1030 conditions in our AISI 1030 yield, tensile and hardness comparison. Looking for AISI 1030 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined AISI 1030 steel parts in-house and inspects them before shipment. |
AISI 1030 As Rolled Designation
| AISI 1030 | |
| Condition | As rolled |
| UNS number | G10300 |
| US name | ASTM 1030, ASTM 1029, ASTM G10290, ASME G10300, ~ASTM M1031, ~ASTM FPB, ~ASTM C2, ~ASTM A-1, ~ASTM 36, ~ASTM 1029, ~ASME G10290 |
| JIS (Japanese) name | ~STPG 410, ~STKM15C, ~STKM15A, ~STKM14C, ~STKM14B, ~STKM14A, ~SPHT 4 |
AISI 1030 As Rolled Typical uses
| General construction, general mechanical engineering, automotive, tools, axles, gears, springs |
AISI 1030 As Rolled Composition detail
| C (carbon) | 0.28 | – | 0.34 | % |
| Fe (iron) | 98.7 | – | 99.1 | % |
| Mn (manganese) | 0.6 | – | 0.9 | % |
| P (phosphorus) | 0 | – | 0.04 | % |
| S (sulfur) | 0 | – | 0.05 | % |
AISI 1030 As Rolled Physical properties
| Density | 7.8 | – | 7.9 | g/cm3 |
AISI 1030 As Rolled Mechanical properties
| Young’s modulus | 208 | – | 216 | GPa |
| Specific stiffness | 26.5 | – | 27.5 | MN.m/kg |
| Yield strength (elastic limit) | 310 | – | 380 | MPa |
| Tensile strength | 495 | – | 610 | MPa |
| Specific strength | 39.5 | – | 48.4 | kN.m/kg |
| Elongation | 25 | – | 39 | % strain |
| Compressive strength | 310 | – | 380 | MPa |
| Flexural modulus | 208 | – | 216 | GPa |
| Flexural strength (modulus of rupture) | 310 | – | 380 | MPa |
| Shear modulus | 80 | – | 85 | GPa |
| Bulk modulus | 161 | – | 176 | GPa |
| Poisson’s ratio | 0.285 | – | 0.295 | |
| Shape factor | 58 | |||
| Hardness – Vickers | 170 | – | 200 | HV |
| Elastic stored energy (springs) | 229 | – | 338 | kJ/m3 |
| Fatigue strength at 10^7 cycles | 261 | – | 303 | MPa |
| Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles | 226 | – | 350 | MPa |
AISI 1030 As Rolled Impact & fracture properties
| Fracture toughness | 49 | – | 78 | MPa.m0.5 |
| Toughness (G) | 11.8 | – | 27.5 | kJ/m2 |
AISI 1030 As Rolled Thermal properties
| Melting point | 1450 | – | 1510 | °C |
| Maximum service temperature | 331 | – | 353 | °C |
| Minimum service temperature | -63 | – | -33 | °C |
| Thermal conductivity | 50 | – | 55 | W/m.°C |
| Specific heat capacity | 465 | – | 505 | J/kg.°C |
| Thermal expansion coefficient | 11 | – | 12.5 | µstrain/°C |
| Thermal shock resistance | 122 | – | 156 | °C |
| Thermal distortion resistance | 4.13 | – | 4.84 | MW/m |
| Latent heat of fusion | 270 | – | 275 | kJ/kg |
AISI 1030 As Rolled Electrical properties
| Electrical resistivity | 16 | – | 19 | µohm.cm |
| Electrical conductivity | 9.07 | – | 10.8 | %IACS |
| Galvanic potential | -0.52 | – | -0.44 | V |
AISI 1030 As Rolled Magnetic properties
| Magnetic type | Magnetic |
AISI 1030 As Rolled Optical, aesthetic and acoustic properties
| Transparency | Opaque | |||
| Acoustic velocity | 5140 | – | 5250 | m/s |
| Mechanical loss coefficient (tan delta) | 8.7e-4 | – | 0.00108 | |
AISI 1030 As Rolled Processing properties
| Metal casting | Unsuitable |
| Metal cold forming | Acceptable |
| Metal hot forming | Acceptable |
| Metal press forming | Acceptable |
| Metal deep drawing | Acceptable |
| Machining speed | 29.6 m/min |
| Weldability Notes: Preheating and post weld heat treatments are required | Good |
| Carbon equivalency | 0.38 – 0.49 |
AISI 1030 As Rolled Durability
| Water (fresh) | Acceptable |
| Water (salt) | Limited use |
| Weak acids | Limited use |
| Strong acids | Unacceptable |
| Weak alkalis | Acceptable |
| Strong alkalis | Limited use |
| Organic solvents | Excellent |
| Oxidation at 500C | Acceptable |
| UV radiation (sunlight) | Excellent |
| Galling resistance (adhesive wear) Notes: Can be used for gears only if hardened. Aluminum bronze is the most suitable mating material to minimize galling. | Limited use |
| Flammability | Non-flammable |
AISI 1030 As Rolled Corrosion resistance
| Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Nitrate, hydroxide, carbonate, ammonia | Not susceptible |
AISI 1030 As Rolled Standards with similar compositions
| China: ML30Mn to GB/T 6478 |
| India: 30C8 to IS 1570/2/1, 35C8 to IS 1570/2/1, C30 to IS 1570/2/1, C30 to IS 6967, C35Mn75 to IS 1570/2/1, CDS-4 to IS 3074 |
| Mexico: 1029 to NMX-B-301, 1030 to NMX-B-201, 1030 to NMX-B-203-SCFI, 1030 to NMX-B-301, 1034 to NMX-B-301, 1035 to NMX-B-203-SCFI, 1035 to NMX-B-301, 1037 to NMX-B-301 |
| Pan America: 1029 to COPANT 333, 1030 to COPANT 330, 1030 to COPANT 331, 1030 to COPANT 333, 1034 to COPANT 333, 1035 to COPANT 330, 1035 to COPANT 331, 1035 to COPANT 333 |
| Sweden: 1550 to SS 141550 |
| UK: 080M30 to BS 970/1 |
| USA: 1029, 1029 to ASTM A29/A29M, 1029 to SAE J403, 1030, 1030 to ASTM A29/A29M, 1030 to ASTM A512-96, 1030 to ASTM A513, 1030 to ASTM A519, 1030 to ASTM A568/A568M, 1030 to SAE J403, 1033, 1033 to ASTM A513, 1033 to ASTM A568/A568M, 1033 to SAE J403, 1034, 1034 to ASTM A29/A29M, 1035, 1035 Class A to ASTM A311/A311M, 1035 to ASTM A29/A29M, 1035 to ASTM A512-96, 1035 to ASTM A513, 1035 to ASTM A519, 1035 to ASTM A568/A568M, 1035 to DoD-F-24669/1, 1035 to FED QQ-W-461H, 1035 to SAE J403, 1037, 1037 to ASTM A29/A29M, 1037 to ASTM A568/A568M, 1037 to SAE J1249, 1037 to SAE J403, C1030 to FED QQ-S-635B, C1030 to FED QQ-S-700D, C1035 to FED QQ-S-635B, C1035 to FED QQ-S-700D, C3 to MIL-S-16788A, CS1030 to MIL-S-11310E, E to MIL-T-20157, G10290 to ASTM A510/A510M, G10290 to ASTM A576-90b, G10300 to ASTM A510/A510M, G10300 to ASTM A576-90b, G10300 to ASTM A830/A830M, G10330 to ASTM A830/A830M, G10340 to ASTM A510/A510M, G10350 to ASTM A510/A510M, G10350 to ASTM A576-90b, G10350 to ASTM A830/A830M, G10370 to ASTM A510/A510M, G10370 to ASTM A576-90b, G10370 to ASTM A830/A830M, MIL-S-3289B to MIL-S-3289B, UNS G10290, UNS G10300, UNS G10300 to UNS, UNS G10330, UNS G10340, UNS G10350, UNS G10350 to UNS, UNS G10370, UNS G10370 to UNS, UNS K02901 |
| Tradenames: CS1030, D-M-E NO. 1, GREDE 34, JESSOP STEEL A-4 (S M-30), NITRIX 1473, V3, V3/1 |