Aluminum 6082 Chemical Composition

Designation
6082, wrought  
UNS numberA96082
EN name EN AW-6082 (EN AW-Al Si1MgMn)
EN number3.2315

Aluminum 6082 Chemical Composition

Al (aluminum)95.2–98.3%
Cr (chromium)0–0.25%
Cu (copper)0–0.1%
Fe (iron)0–0.5%
Mg (magnesium)0.6–1.2%
Mn (manganese)0.4–1%
Si (silicon)0.7–1.3%
Ti (titanium)0–0.1%
Zn (zinc)0–0.2%
Other0–0.15%


MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey