Aluminum 6082 Similar Compositions

Designation 6082, wrought   UNS number A96082 EN name EN AW-6082 (EN AW-Al Si1MgMn) EN number 3.2315 Aluminum 6082 Equivalent Grades Australia: 6082 to AS 2848.1 Austria: AlMgSi1 to ONORM M3430 Europe: EN AW-6082 to CEN EN 573-3, EN AW-6082A to CEN EN 573-3 France: 6082 to NF A50-411 Germany: 3.2315/AlMgSi1 to DIN 1725-1 Hungary: AlMgSi1 … Continue reading Aluminum 6082 Similar Compositions