Aluminum 6082 T6 Mechanical Properties
Designation 6082, wrought Condition T6 (Solution heat-treated and artificially aged) UNS number A96082 EN name EN AW-6082 (EN AW-Al Si1MgMn) EN number 3.2315 Aluminum 6082 T6 Mechanical Properties Young’s modulus 70 – 74 GPa Specific stiffness 25.9 – 27.5 MN.m/kg Yield strength (elastic limit) 240 – 280 MPa Tensile strength 295 – 344 MPa … Continue reading Aluminum 6082 T6 Mechanical Properties