Aluminum 6082 T4 Mechanical Properties
Designation 6082, wrought Condition T4 (Solution heat-treated and naturally aged to a substantially stable condition) UNS number A96082 EN name EN AW-6082 (EN AW-Al Si1MgMn) EN number 3.2315 Aluminum 6082 T4 Mechanical Properties Young’s modulus 70 – 74 GPa Specific stiffness 25.9 – 27.5 MN.m/kg Yield strength (elastic limit) 115 – 134 MPa Tensile … Continue reading Aluminum 6082 T4 Mechanical Properties