Aluminum 6082 Similar Compositions

Designation
6082, wrought  
UNS numberA96082
EN name EN AW-6082 (EN AW-Al Si1MgMn)
EN number3.2315

Aluminum 6082 Equivalent Grades

Australia: 6082 to AS 2848.1
Austria: AlMgSi1 to ONORM M3430
Europe: EN AW-6082 to CEN EN 573-3, EN AW-6082A to CEN EN 573-3
France: 6082 to NF A50-411
Germany: 3.2315/AlMgSi1 to DIN 1725-1
Hungary: AlMgSi1 to MSZ 3714/1
India: 64430 to IS 733, 64430 to IS 736, HG30 to IS 739
International: AlSi1Mg to ISO/R 827, AlSi1Mg to ISO/R 829, AlSi1Mg to ISO/TR 2778, AlSi1MgMn to ISO 209-1
Norway: 17305 to NS 17305
Sweden: 4212-00 to SIS 144212, 4212-02 to SIS 144212, 4212-04 to SIS 144212, 4212-10 to SIS 144212
UK: 6082 to BS 1471, 6082 to BS 1472, 6082 to BS 1473, 6082 to BS 1474
USA: 6082, 6082A, UNS A96082
Yugoslavia: 3.4552.00/AlSi1Mg to JUS C.C2.100
Tradenames: ALCAN B51S, ALCOA 920, ALMGSI 1 (410) 6100, ANTICORODAL-090, ANTICORODAL-110, ANTICORODAL-112, BAW 6082, IMPALCO M39/2, KAISER ALLOY 6082 T4, KAISER ALLOY 6082 T6


MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey