AISI 1020 Carbon Steel Similar and Equivalent Grades
| Australia: S1020 to AS 1442, S1020 to AS 1443, S1020 to AS 1446 |
| Austria: C22SP to ONORM M3167 |
| China: CRB650 to GB 13788, ML20Al to GB/T 6478, Q235 to GB/T 3524 |
| Hungary: B38X to MSZ 500 |
| India: 17C5 to IS 8053, ERW-3 to IS 3074, Grade 8 to IS 7887, Grade 8 to IS 8952 |
| International: CC21A to ISO 4954 |
| Italy: C21 to UNI 6922, CB20FF to UNI 7356 |
| Japan: SWRCH20A to JIS G3507, SWRM 20 to JIS G3505 |
| Mexico: 1020 to NMX-B-301, MT1020 to NMX-B-201, MT1020 to NMX-B-203-SCFI |
| Pan America: 1020 to COPANT 330, 1020 to COPANT 331, 1020 to COPANT 333 |
| South Korea: SWRCH20A to KS D 3592, SWRM 20 to KS D 3554 |
| Spain: 18KA-DF to UNE 36032, 20KA-DF to UNE 36032, F.7516 to UNE 36032, F.7517 to UNE 36032 |
| UK: 040A20 to BS 970/1 |
| USA: 1020, 1020 to ASTM A29/A29M, 1020 to ASTM A512-96, 1020 to ASTM A513, 1020 to ASTM A519, 1020 to ASTM A568/A568M, 1020 to DoD-F-24669/1, 1020 to FED QQ-S-635B, 1020 to FED QQ-S-698, 1020 to FED QQ-W-461H, 1020 to MIL-S-7952A, 1020 to MIL-T-3520, 1020 to SAE J403, 1023, 1023 to ASTM A513, 1023 to ASTM A568/A568M, 1023 to SAE J403, 5032 to AMS 5032E, C2 to MIL-S-16788A, CS1020 to MIL-S-11310E, G10200 to ASTM A510/A510M, G10200 to ASTM A576-90b, G10200 to ASTM A830/A830M, G10200 to MIL-S-46059, Grade A to ASTM A595, Grade B to ASTM A730, M1020, M1020 to ASTM A29/A29M, M1020 to ASTM A575-96, M1020 to SAE J403, MT1020 to ASTM A512-96, MT1020 to ASTM A513, MT1020 to ASTM A519, MT1020 to ASTM A787, UNS G10200, UNS G10200 to UNS, UNS G10230, UNS K01900, UNS K02000, UNS K02004, UNS K11900 |
| Tradenames: |
| ASCOMETAL XC18, B-W STANDARDIZED, CS1020, MARREL M5, POMPEY FFC 2, TOLEDO 15, UNION MC QUAID-EHN, V2 |
AISI 1020 Designation
| AISI 1020 | |
| UNS number | G10200 |
| US name | ASTM MT1020, ASTM M1020, ASTM 1020, ASME G10200, ASME G10170, ASME 1017, ~SAE 040 X, Y, Z, ~SAE 035S, ~SAE 035C, ~SAE 035B, ~SAE 035A, ~SAE 035 X, Y, Z, ~ASTM A836, ~ASTM 1018 Class A, ~ASME G10210, ~ASME G10180, ~ASME 1021 |
| EN name | S240GP, ~P355NB, ~P310NB, ~HS15 |
| EN number | ~1.0021 |
| ISO name | ~E235 Quality A, ~CE20E4, ~CC21A |
| GB (Chinese) name | ~ML20Al, ~ML18Mn |
| JIS (Japanese) name | SWRM 20, SWRCH20A, SG 255, ~SWRCH18A, ~STKM12C, ~STKM12B, ~STKM12A, ~SPHT 2 |
MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey