AISI 1020 Carbon Steel Annealed Mechanical Properties
AISI 1020 Annealed Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 265 – 325 MPa Tensile strength 355 – 435 MPa Specific strength 33.8 – 41.4 kN.m/kg Elongation 28 – 43 % strain Compressive strength 265 – 325 MPa Flexural modulus 205 – 215 GPa … Continue reading AISI 1020 Carbon Steel Annealed Mechanical Properties