AISI 1020 Carbon Steel As Rolled Mechanical Properties

AISI 1020 As Rolled Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 295 – 365 MPa Tensile strength 395 – 500 MPa Specific strength 37.6 – 46.5 kN.m/kg Elongation 28 – 43 % strain Compressive strength 295 – 365 MPa Flexural modulus 205 – 215 … Continue reading AISI 1020 Carbon Steel As Rolled Mechanical Properties