AISI 1020 Carbon Steel Normalized Mechanical Properties
AISI 1020 Normalized Mechanical Properties Young’s modulus 205 – 215 GPa Specific stiffness 26.1 – 27.4 MN.m/kg Yield strength (elastic limit) 310 – 350 MPa Tensile strength 395 – 490 MPa Specific strength 39.5 – 44.6 kN.m/kg Elongation 28 – 43 % strain Compressive strength 310 – 350 MPa Flexural modulus 205 – 215 GPa … Continue reading AISI 1020 Carbon Steel Normalized Mechanical Properties