AISI 1020 Carbon Steel Annealed Mechanical Properties

AISI 1020 Steel Investment Casting Sand Casting Machining Turning Manufacturing CNC Milling Supplier Company in Turkey Turkiye

AISI 1020 Annealed Mechanical Properties

Young’s modulus205–215GPa
Specific stiffness26.1–27.4MN.m/kg
Yield strength (elastic limit)265–325MPa
Tensile strength355–435MPa
Specific strength33.8–41.4kN.m/kg
Elongation28–43% strain
Compressive strength265–325MPa
Flexural modulus205–215GPa
Flexural strength (modulus of rupture)265–325MPa
Shear modulus79–84GPa
Bulk modulus158–175GPa
Poisson’s ratio0.285–0.295 
Shape factor61   
Hardness – Vickers110–130HV
Elastic stored energy (springs)169–249kJ/m^3
Fatigue strength at 10^7 cycles207–240MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles180–277MPa

AISI 1020 Annealed Impact & fracture properties

Fracture toughness42–67           MPa.m^0.5
Toughness (G)8.78–20.5kJ/m^2

AISI 1020 Designation

AISI 1020
Condition: Annealed
UNS numberG10200
US nameASTM MT1020, ASTM M1020, ASTM 1020, ASME G10200, ASME G10170, ASME 1017, ~SAE 040 X, Y, Z, ~SAE 035S, ~SAE 035C, ~SAE 035B, ~SAE 035A, ~SAE 035 X, Y, Z, ~ASTM A836, ~ASTM 1018 Class A, ~ASME G10210, ~ASME G10180, ~ASME 1021
EN nameS240GP, ~P355NB, ~P310NB, ~HS15
EN number~1.0021
ISO name~E235 Quality A, ~CE20E4, ~CC21A
GB (Chinese) name~ML20Al, ~ML18Mn
JIS (Japanese) nameSWRM 20, SWRCH20A, SG 255, ~SWRCH18A, ~STKM12C, ~STKM12B, ~STKM12A, ~SPHT 2

MODULUS METAL
Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Foundry in Turkey, Plastic Injection Molding in Turkey, Press Bending ( Press Brake) Products in Turkey, Laser and Plasma Cutting in Turkey, Welded Construction in Turkey, Heat Treated, CNC Machined Products Manufacturer in Turkey, Additive Manufacturing and 3D Printing in Turkey, Quality Enginering and Inspection Service in Turkey, Manufacturing Inspection Service in Turkey, Quality Engineering and Supplier Quality Engineering Service in Turkey, Supplier Quality Control and Inspection Service in Turkey, Resident Engineering Services in Turkey