Aluminum 356.0 sand cast F General Information
| General Information | |
|---|---|
| Designation | 356.0 (Aluminum Association) |
| Condition | F (As-fabricated) |
| UNS Number | A03560 |
| EN Number | EN AC-42000 / EN AC-Al Si7Mg |
| Aluminum 356.0 sand cast F General Information |
Aluminum 356.0 sand cast F Typical Uses
| Typical Uses |
|---|
| High strength alloy for the automotive industry |
| Space frames |
| Wheels |
| Axle and differential housings |
| Pump |
| Meter |
| Differential housings |
| Intake manifolds |
| Electronic cases |
| Fuel pumps |
| Aluminum 356.0 sand cast F Typical Uses |