Aluminum 356.0 sand cast F Mechanical Properties
| Property | Range |
|---|---|
| Young’s Modulus | 71.5 – 74.5 GPa |
| Specific Stiffness | 26.6 – 27.8 MN.m/kg |
| Yield Strength (Elastic Limit) | 118 – 130 MPa |
| Tensile Strength | 164 – 180 MPa |
| Specific Strength | 43.8 – 48.5 kN.m/kg |
| Elongation | 6 – 7.2 % strain |
| Compressive Strength | 118 – 130 MPa |
| Flexural Modulus | 71.5 – 74.5 GPa |
| Flexural Strength (Modulus of Rupture) | 124 – 136 MPa |
| Shear Modulus | 26.7 – 28.2 GPa |
| Bulk Modulus | 66.9 – 76.6 GPa |
| Poisson’s Ratio | 0.322 – 0.338 |
| Shape Factor | 38 |
| Hardness (Vickers) | 86 – 96 HV |
| Elastic Stored Energy (Springs) | 95.1 – 116 kJ/m^3 |
| Fatigue Strength at 10^7 cycles | 98.9 – 111 MPa |
| Fatigue Strength Model (Stress Range) | 94.1 – 117 MPa |