Aluminum, 356.0, sand cast, F | Composition
Aluminum 356.0 sand cast F Composition Property Value Compositional Summary Al90-93 / Si6.5-7.5 / Mg0.2-0.45 Impurities Fe < 0.6, Mn < 0.35, Zn < 0.35, Cu < 0.25, Ti < 0.25, Other < 0.15 Material Family Metal (non-ferrous) Base Material Al (Aluminum) Aluminum 356.0 sand cast F Composition Detail Element Range (%) Al (Aluminum) 90.1 … Continue reading Aluminum, 356.0, sand cast, F | Composition