Aluminum 356.0 sand cast F Composition
| Property | Value |
|---|---|
| Compositional Summary | Al90-93 / Si6.5-7.5 / Mg0.2-0.45 |
| Impurities | Fe < 0.6, Mn < 0.35, Zn < 0.35, Cu < 0.25, Ti < 0.25, Other < 0.15 |
| Material Family | Metal (non-ferrous) |
| Base Material | Al (Aluminum) |
Aluminum 356.0 sand cast F Composition Detail
| Element | Range (%) |
|---|---|
| Al (Aluminum) | 90.1 – 93.3 |
| Cu (Copper) | 0 – 0.25 |
| Fe (Iron) | 0 – 0.6 |
| Mg (Magnesium) | 0.2 – 0.45 |
| Mn (Manganese) | 0 – 0.35 |
| Si (Silicon) | 6.5 – 7.5 |
| Ti (Titanium) | 0 – 0.25 |
| Zn (Zinc) | 0 – 0.35 |
| Other | 0 – 0.15 |