Aluminum, 356.0, sand cast, F | Mechanical Properties
Aluminum 356.0 sand cast F Mechanical Properties Property Range Young’s Modulus 71.5 – 74.5 GPa Specific Stiffness 26.6 – 27.8 MN.m/kg Yield Strength (Elastic Limit) 118 – 130 MPa Tensile Strength 164 – 180 MPa Specific Strength 43.8 – 48.5 kN.m/kg Elongation 6 – 7.2 % strain Compressive Strength 118 – 130 MPa Flexural Modulus … Continue reading Aluminum, 356.0, sand cast, F | Mechanical Properties