Aluminum, 356.0, sand cast, F | Equivalent Grades

Standards with similar compositions of Aluminum 356.0 sand cast F

Country/RegionStandard
AustraliaDA601 to AS 1874
BelgiumAlSi7 to NBN P21-101
CanadaSG70N to CSA HA.10, SG70N to CSA HA.9, SG70P to CSA HA.10, SG70P to CSA HA.9
Czech Republic424332 to CSN
EuropeEN AC-42000 to CEN EN 1706
FranceA-S7G to NF A50-702
India4450 to IS 202 or 617
InternationalAlSi7Mg(Fe) to ISO 3522
JapanAC4C to JIS H5202, AC4C.1 to JIS H2211
Norway17525 to NS 17525
RussiaAL9 to GOST 2685
South AfricaAl-Si7Mg0.3 to SABS 991, SA14(Al-Si7MgA) to SABS 989
SpainL-2651 to UNE 38-203, L-2651 to UNE 38-267
UKLM25 to BS 1490
USA356, 356 to ASTM B108, 356 to ASTM B26/B26M, 356 to ASTM B618, 356.1, 356.1 to ASTM B179, A03560 to SAE J452, A356.0 to ASTM B26/B26M, A356.0 to MIL A-21180C, UNS A03560, UNS A03561

Tradenames of Aluminum 356.0 sand cast F

Tradenames
A356
ALLCAST 46
ALLCAST 46A
AS 601

MODULUS METAL
Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey