General Information for Aluminum 336.0 (Permanent Mold Cast, T65)
| Attribute | Value |
|---|---|
| Designation | 336.0 (Aluminum Association) |
| Condition | T65 (Solution heat-treated and artificially aged) |
| UNS Number | A03360 |
| General Information for Aluminum 336.0 (Permanent Mold Cast, T65) |
Typical Uses for Aluminum 336.0 (T65)
| Application |
|---|
| High-temperature alloy: |
| – Pistons |
| – Cylinder heads |
| – Gear housings |
| – Other engine parts |