Aluminum, 336.0, permanent mold cast, T65 | Mechanical Properties
Mechanical Properties for Aluminum 336.0 (T65) Property Value Range Unit Young’s Modulus 72.5 – 75.5 GPa Specific Stiffness 26.7 – 27.9 MN·m/kg Yield Strength (Elastic Limit) 281 – 311 MPa Tensile Strength 309 – 341 MPa Specific Strength 103 – 115 kN·m/kg Elongation 1 – 2 % strain Compressive Strength 281 – 311 MPa Flexural … Continue reading Aluminum, 336.0, permanent mold cast, T65 | Mechanical Properties
Copy and paste this URL into your WordPress site to embed