Standards with Similar Compositions for Aluminum 336.0 (T65)
Country
Standard
Canada
SN122 to CSA, SN122 to CSA HA.10, SN122 to CSA HA.3
Italy
6250/G-AlSi12.7NiMgCu to UNI
Spain
L-2550 to UNE 38-203
USA
336, 336 to ASTM B108, 336.1, 336.1 to ASTM B179, 336.2, 336.2 to ASTM B179, A03360 to SAE J452, A332.1 to QQ A-371F, A332.2 to QQ A-371F, UNS A03360, UNS A03361, UNS A03362
Standards with Similar Compositions for Aluminum 336.0 (T65)
MODULUS METAL | ALUMINUM CASTING FOUNDRY IN TURKEY Aluminium Sand Casting in Turkey, Permanent Mold Casting in Turkey, Gravity Die Casting in Turkey, Pressure Die Casting in Turkey, High-Pressure Die Casting in Turkey, Investment Casting in Turkey, Plaster Casting in Turkey, Heat Treated and CNC Machined Products Manufacturer in Turkey