Composition Summary for Aluminum 336.0 (T65)

AttributeValue
Compositional SummaryAl79-86 / Si11-13 / Ni2-3 / Cu0.5-1.5 / Mg0.7-1.3 (impurities: Fe<1.2, Mn<0.35, Zn<0.35, Ti<0.25, Other<0.05)
Material FamilyMetal (non-ferrous)
Base MaterialAluminum (Al)
Composition Summary for Aluminum 336.0 (T65)

Compositional Details for Aluminum 336.0 (T65)

ElementRange (% by weight)
Aluminum (Al)79 – 86
Silicon (Si)11 – 13
Nickel (Ni)2 – 3
Copper (Cu)0.5 – 1.5
Magnesium (Mg)0.7 – 1.3
Iron (Fe)0 – 1.2
Manganese (Mn)0 – 0.35
Zinc (Zn)0 – 0.35
Titanium (Ti)0 – 0.25
Other0 – 0.05