Aluminum, 336.0, permanent mold cast, T65 | Composition
Composition Summary for Aluminum 336.0 (T65) Attribute Value Compositional Summary Al79-86 / Si11-13 / Ni2-3 / Cu0.5-1.5 / Mg0.7-1.3 (impurities: Fe<1.2, Mn<0.35, Zn<0.35, Ti<0.25, Other<0.05) Material Family Metal (non-ferrous) Base Material Aluminum (Al) Composition Summary for Aluminum 336.0 (T65) Compositional Details for Aluminum 336.0 (T65) Element Range (% by weight) Aluminum (Al) 79 – 86 … Continue reading Aluminum, 336.0, permanent mold cast, T65 | Composition